铁氟龙, 氟橡胶, 铁氟龙FEP, PVDF法国阿科玛9000HD, ETFE日本旭硝子C-88AX, PFA美国杜邦340, PA66/F/PTFE美国液氮RFL-403, PA66/PTFE美国液氮RL-4040, POM/PTFE基础创新塑料KL004
| Fluoroplex CG 35 - GMP | |||
| Polytetrafluoroethylene | |||
| 35% Coke\Graphite | |||
| Product Description | |||
| Fluoroplex CG 35 - GMP is a Polytetrafluoroethylene (PTFE) product filled with 35% coke\graphite. It can be processed by injection molding or sintering and is available in Latin America or North America. | |||
| General | |||
| Filler / Reinforcement | Coke\Graphite, 35% Filler by Weight | ||
| Features | Good Flow | ||
| Processing Method | Injection Molding | Sintering | |
| Physical | Nominal Value | Unit | Test Method |
| Specific Gravity | 1.99 to 2.07 | g/cm³ | Internal Method |
| Apparent Density | 0.52 to 0.62 | g/cm³ | Internal Method |
| Particle Size Distribution - d50 | 468.0 to 728.0 | µm | Internal Method |
| Shrinkage - Sintering | 0.80 to 1.8 | % | Internal Method |
| Hardness | Nominal Value | Unit | Test Method |
| Shore Hardness (Shore D) | 65 to 72 | Internal Method | |
| Elastomers | Nominal Value | Unit | Test Method |
| Tensile Strength | 12 | MPa | Internal Method |
| Tensile Elongation (Break) | 14 | % | Internal Method |
| Additional Information | Nominal Value | Unit | Test Method |
| Flow Time - 50 grams | 3.0 to 4.0 | sec | Internal Method |
| Sintering Temperature - Maximum | 365 | °C | |
| Code: 010003002 | |||
| Injection | Nominal Value | Unit | |
| Mold Temperature | 21.0 to 25.0 | °C | |
| Injection Pressure | 63.7 to 73.5 | MPa | |